Affiliation:
1. National Engineering Research Center for Ionic Rare Earth
2. Université du Québec
Abstract
Sc0.88Lu0.05(V1-xPx)O4:Eu3+0.07(0≤x≤0.5) phosphors were synthesized by co-precipitation method. The structure, morphology and luminescence spectra of samples were investigated by XRD, SEM and fluorescence spectrophotometer, respectively. The samples doped with Eu3+, Lu3+and PO43-can maintain the body-centered tetragonal structure of ScVO4and the morphology essentially remains unchanged with slight agglomeration. The excitation spectrum intensity of Sc0.88Lu0.05(V1-xPx)O4:Eu3+0.07increase within the near UV excitation (360-410nm). The optimum doping concentration of PO43-is 0.2(x value), and the maximum emission intensity of Sc0.88Lu0.05(V0.8P0.2)O4:Eu3+0.07is about 35 % higher than the Sc0.88Lu0.05VO4:Eu3+0.07under 365 nm excitation. Decay curve of5D0state for as-prepared samples fits the single order exponential behavior, the lifetime of5D0increase first and then decrease with the increase of PO43-doping concentration. The internal quantum efficiency is up to 66.73% under 365nm excitation, When the temperature rises to 200°C, the emission intensity maintains 79.3% of that in the room temperature. Sc0.88Lu0.05(V0.8P0.2)O4:Eu3+0.07phosphor shows high internal quantum efficiency and thermal stability, which is suitable for the UV-pumped white LED as red phosphor.
Publisher
Trans Tech Publications, Ltd.
Subject
Mechanical Engineering,Mechanics of Materials,Condensed Matter Physics,General Materials Science
Reference15 articles.
1. J. ZHANG, Y. YANG, Y. LIU, C. MI, G. LI, B. HAN, Y. ZHANG, H. -J. SEO. J Am Ceram Soc., 98(2015) 1567-1573.
2. A. Setlur, The Electrochemical Society Interface, 16 (2009) 32.
3. L. XIA, X. YE, X. PAN, W. YOU, Q. XIAO, Z. LI. J Chin Ceram Soc., 45(2017) 410–415.
4. Z. WANG, H. LIANG, J. WANG. Materials Research Bulletin, 43(2008) 907-911.
5. Z. ZHANG, Q. HUANG, X. ZHAO. PHYS. STATUS SOLIDI A, 206(2009) 2839-2843.