Abstract
PMMA/PS copolymers were synthesized by radical polymerization techniques. And the 1H NMR results illustrate that the molar contents of PMMA are respectively 19%, 53%, 69% and 84%. The coatings of those PMMA/PS copolymers were prepared by spin-coating. The surface structures and protein resistance of copolymer coatings were investigated respectively by AFM and BSA absorption experiment. It is showed that the copolymer coating surfaces have micro-phase separation structure. Furthermore, with the increase in the PMMA content, the surface pattern changes from interpenetration network pattern to island structure that the PMMA-rich phase surrounded by the PS-rich phase. In addition, all coatings prepared in this study, especially the coating with PMMA content of 69%, have good resistance to BSA protein.
Publisher
Trans Tech Publications, Ltd.
Reference15 articles.
1. A. A. Gavrilov, Y. V. Kudryavtsev and P. G. Khalatur: Chem. Phys. Lett., 2011, 503, 277-282.
2. D. C. Pham, K. Na, S. Piao, S. Yang, J. Kim and E.S. Yoon: Surf. Eng., 2011, 27, 286-293.
3. H. G. Ni, J. Gao, X. H. Li, Y. Y. Hu, D. H. Yan, X. Y. Ye and X. P. Wang: J. Colloid Interface Sci., 2012, 365, 260-267.
4. L. Y. Xie, F. Hong, C. X. He, C. F. Ma, J. H. Liu, G. Z. Zhang, and C. Wu: Polym., 2011, 52, 3738-3744.
5. H. Kaczmarek and H. Chaberska: Appl. Surf. Sci., 2009, 255, 6729-6735.