Abstract
Pure lead titanate (PbTiO3) and Sn doped PbTiO3 solid solution were prepared by sol-gel technique. The sol was prepared by mixing stable solutions of Pb-citrate, Sn-and Ti (OC4H9)4 precursors. The structure and particle size and morphology of PbTiO3 powder were characterized by XRD, and the results shows that the precursors decomposed and forms pure phase after heating at 973 K and 1073 K for 2 h. Influence of different factors on PbTiO3 gel doped with Sn was discussed. It is found that higher synthesis temperature is needed to prepare Sn doped PbTiO3 solid solutions.
Publisher
Trans Tech Publications, Ltd.
Reference7 articles.
1. M. L. Calzada, J. de Frutos, Chemical processing and microstructure of piezoelectric lead titanate ceramics, Journal of Materials Science: Materials in Electronics, Vol. 4 1 (1993) 83.
2. S.J. Zhang, S. Taylor, F. Li. Piezoelectric property of relaxor-PbTiO3 crystals under uniaxial transverse stress, Applied Physics Letters, Vol. 102 17 (2013) 2902.
3. W. Zheng, G. Xu, Z. Ren et al, Glucose modified hydrothermal synthesis of perovskite oxide nanocrystals, Rare Metal Materials Engineering, Vol. 41 3 (2012) 129.
4. L. Liu, R. Zuo, Q. Sun, et al, Structure and electrical properties of Mn doped Bi (Mg1/2Ti1/2) O3-PbTiO3 ferroelectric thin films, Applied Surface Science, 268 (2011) 327.
5. A. Pelaiz-Barranco, Y. Mendez-Gonzalez, D. C. Arnold, et al, Incorporation of lanthanide ions in lead titanate, Journal of Materials Science, Vol. 47 2 (2012) 1094.
Cited by
1 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献