Affiliation:
1. Academy of Armored Forces Engineering
2. Institute of Chemical Defence
Abstract
The preparation of electrolyte and the technical flow were summarized, the chromium based nanodiamond composite coating was prepared by composite plating process. The metallography structure of plating layer was characterzied, and the hardness, the element of plating layer were tested, the test results and reaction principle were discussed. It was found that the addition of nanodiamond increased the hardness of the coatings. When the concentration of DND in electrolyte is 2.0-3.0g/L,the plating time is about 15-20min, the maximum hardness was obtained.
Publisher
Trans Tech Publications, Ltd.
Reference9 articles.
1. Tong Guo, Zhang San-yuan. Composite coatings [M]. Tianjin: Tianjin University Press, 1991. (In Chinese ).
2. Marco Musiani, Electrodepositon of composite: an expanding subject in electrochemical materials science [J], Electrochimical Acta, 2000, 45: 3397-3402.
3. El SharifM, Chisholm C V. Characteristics of electrodeposited chromium [J]. Trans MF., 1997, 75 (6): 208-212.
4. Jamese H, Lindsay. Decorative and hard chromium plating [J]. Planting and Surface Finishing, 2004, (8): 16-17.
5. Mandich NV, Dennis J K. Codepositon of nano-diamond with chromium [J]. Metal Finishing, 2001, 99 (66): 117-119.
Cited by
1 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献