Pure Fe3Al and Fe3Al+4%Cr alloys were corroded at 1000 °C for up to 200 h in N2-0.1%H2S-mixed gas in order to study their corrosion behavior in H2S-containing atmosphere. The formed scales consisted primarily of α-Al2O3, FeAl2O4, and Fe2O3. In these oxide scales, hydrogen and sulfur dissolved according to the reaction; H2S→2H+S. Corrosion products of Cr were not identified in the scales from the XRD analysis, indicating that Cr dissolved in the oxide scales. Fe3Al+4%Cr alloy displayed poorer corrosion resistance than Fe3Al alloy, indicating that chromium accelerated the corrosion rates of Fe3Al alloys.