The microstructure, toughness, hardness and wear resistance of Fe-B-C cast wear-resistant alloy were studied. The results indicate that, the as-cast Fe-B-C alloy comprises pearlite, ferrite and eutectic phase Fe2 (B, C), and that, with increasing boron and carbon contents, the boride volume fraction (BVF) and macrohardness increase; furthermore, when boron content increases from about 0.5 wt.% to 2.0 wt.%, the increase trend of the macrohardness will become smaller with increasing the carbon content. The results also indicate that, after heat-treatment, the Fe2 (B, C) becomes coarser than that as cast condition, and the boron content has less effect on the martensite hardness at the same carbon content; with increasing boron and carbon contents, the hardness of the samples increases and inversely the toughness decreases. At a lower BVF, the matrix plays a dominant role on the impact toughness of Fe-B-C alloy; however, at a higher BVF, the BVF plays a dominant role. The wear test results indicate that, with increasing the boron and carbon contents, the weight loss of the samples decreases, namely, the increase of wear resistance.
Publisher
Trans Tech Publications, Ltd.
Subject
Mechanical Engineering,Mechanics of Materials,General Materials Science
Cited by
8 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献