Abstract
Zn (II)/SiMCM-41 and Fe (III)/SiMCM-41 showed high activity in disposal of CCl4into diphenyl carbonate (DPC) in presence of CO2at low temperature, due to Zn (II) and Fe (III) have zero Ligands Field Stabblized Energy (LFSE) and strong Lewis acid. Metal ions were immobilized onto the wall of Si-MCM-41, which keep metal cation leaching from catalyst during reaction