Affiliation:
1. Kunming University of Science and Technology
Abstract
Poly-di (bis-dimethoxy-ethyl) amine phosphazene was synthesized by nucleophilic substitution reaction with bis (dimethoxy ethyl) amine and conductive polymer materials were manufactured by compositing of the lithium salt and polyphosphazene. The results show that: Td10=503K, the maximum decomposition rate was at 653K. When the mol Li+/ repeat unit was 1.5, the conductivity of polyphosphazene composite conductive material comes up to 4.21×10-8S/cm.
Publisher
Trans Tech Publications, Ltd.
Reference9 articles.
1. I. Manners: Ann. Rep. Prog. Chem. Sect. A, Vol. 88(1991), p.77.
2. B. Martin: European Polymer Journa1, 35(1999), p.581.
3. H. R. Allcock: C & EN, 18(1985), p.22.
4. H. R. Allcock, in: Phosphezene high polymers in comprehensive polymer science, edtied by S. G. Allen and J. C. Bevington, Pergamon press(1989).
5. C. A. Reed, J. P. Taylor, K. S. Guigley, et al: Polym Eng & Sci, 2 (2000), p.465.