Peeling along the interface between FRP and concrete under fatigue load is the common failure pattern for the RC structures strengthened with FRP. In this paper, five groups specimens were subjected to fatigue load to study the fatigue mechanism for bonding interface between carbon fiber laminate (CFL) and concrete. The Δσ~N curves for the bonding interface were derived from the experiments, the laws of strains and slip on interface were analyzed in this paper.
Publisher
Trans Tech Publications, Ltd.
Reference11 articles.
1. Meier U, Deuring M, Meier H, Schwegler G. Strengthening of structures with CFRP laminates: research and applications in Switzerland. In: Neale KW, Labossière P, editors. Advanced composite materials in bridges and structures. Montreal, Canada: Canadian Society for Civil Engineering. (1992).
2. Neale KW, Labossière P. State-of-the-art report on retrofitting and strengthening by continuous fibre in Canada. Non-metallic reinforcement for concrete structure. Japan Concrete Institute. (1997) 25–39.
3. Varastehpour H, Hamelin P. Strengthening of concrete beams using fiberreinforced plastics. Mater Struct, RILEM. 30 (1997) 160–6.
4. Inoue S., Nishibayashi S., Yoshino A., et al. Strength and deformation characteristics of reinforced concrete beam strengthened with carbon fiber-reinforced plastics plate under static and fatigue loading [J]. Journal of the Society of Materials Science. (1994).
5. Barnes R. A., Mays G. C. Fatigue performance of concrete beams strengthened with CFRP plates [J]. J Compos for Constr. (1999) 63-72.
Cited by
2 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献