Abstract
This paper describes the deposition of PZT thin films on soda-lime glass substrate with ITO bottom electrode by CSD (Chemical Solution Deposition). The transmittance of the obtained PZT thin film on ITO/glass substrate was about 60 % in the visible light region. The deposited transparent PZT thin film exhibited the ferroelectricity of Pr=36.3 μC/cm2 and Ec=71.3 kV/cm. In addition, the piezoelectric property of the resultant PZT thin film was relatively large and exhibited the measured effective d33 of 120 pC/N after the polarization.
Publisher
Trans Tech Publications, Ltd.
Subject
Mechanical Engineering,Mechanics of Materials,General Materials Science
Reference5 articles.
1. Desheng Fu, Kazuyuki Suzuki, Kazuki Kato and Hisao Suzuki, Appl. Phys. Let. 82(13) pp.2130-2132 (2003).
2. Koji Yamakawa, Keitaro Imai, Osamu Arisumi, Tsunetoshi Arikado, Masaki Yoshioka, Tatsushi Owada and Katsuya Okumura, Jpn. J. Appl. Phys., 41 pp.2630-2634, (2002).
3. Katsunori Noritake, Takashi Matsukawa, Meishoku Koh, Ken-ichi Hara, Makoto Goto and Iwao Ohdomari, Jpn. J. Appl. Phys., 31 pp. L771-L773, (1992).
4. Hisao Suzuki, Mohamed Baijuri Othman, Kenji Murakami, Shoji Kaneko and Takashi Hayashi, Jpn. J. Appl. Phys., 35 pp.4896-4899 (1996).
5. Desheng Fu, Hisao Suzuki, Takeshi Ogawa and Kenji Ishikawa, Appl. Phys. Lett., 80(13), pp.3572-3574 (2002) 1 10 100 200 400 600 loading unloading d33 (pC/N) Time (second).
Cited by
7 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献