Abstract
Effect of microstructure of silicon nitride on the fracture toughness, KIc evaluated by the IF
method was studied with various indentation loads ranging from 49 N to 490 N, since practical
assessment of fracture toughness of small Si3N4 parts is needed in the ceramic ball bearing market.
The plot of KIc against the as-indented crack length revealed the rising R-curve behavior for the coarse
Si3N4 and slight R-curve for the fine Si3N4. By comparing KIc estimated from the SEPB and IF
methods using 4 different equations, it was revealed that the IF equation which gave the nearest value
to KIc from SEPB was different depending on the microstructures. These results were discussed in
conjunction with their R-curve behavior and the effective crack length in the SEPB specimens.
Publisher
Trans Tech Publications, Ltd.
Subject
Mechanical Engineering,Mechanics of Materials,General Materials Science
Reference10 articles.
1. B.R. Lawn, A.G. Evans, and D.B. Marshall: J. Am. Ceram. Soc. Vol. 64 (1981), p.539.
2. H. Awaji, T. Yamada, and H. Okuda: J. Ceram. Soc. Jpn. Vol. 99 (1991), p.417.
3. G. Pezzotti, K. Niihara and T. Nishida: J. Testing and Evaluation Vol. 21 (1993), p.358.
4. S.R. Choi and J.A. Salem: J. Am. Ceram. Soc. Vol. 77 (1994), p.1042.
5. J. Yang, T. Sekino and K. Niihara: J. Mater. Sci. Vol. 34 (1999), p.554.
Cited by
4 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献