Abstract
The adhesive and wear properties of ITO thin film have been investigated using the scratch and wear
tests. ITO thin film was fabricated on glass substrate using RF magnetron sputter and strip lines were
formed by selective etching. In the scratch test, the normal load on WC micro-blade was increased
and kept constant as it was drawn over the films. In the wear test, sapphire, SUS and WC balls slided
repeatedly on the films with the constant normal load. During the scratch and wear, the ESR and the
acoustic signal were monitored and recorded. In order to study the adhesive and wear properties of
ITO thin films, it was desirable to use the ESR rather than the acoustic signal. From the change in the
ESR, it was possible to measure the critical load to cut through ITO film completely and the critical
number of sliding to wear ITO film completely.
Publisher
Trans Tech Publications, Ltd.
Subject
Mechanical Engineering,Mechanics of Materials,General Materials Science
Cited by
4 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献