Abstract
The viscosity of an electrorheological fluid (ER fluid) increases with an increase in the
intensity of an electric field. In the case of ER fluid-assisted micro polishing the workpiece needs to
be a conductive material such as tungsten carbide and the gap between the workpiece and the
polishing tool, which both act as electrodes, must be the same size as the abrasive grain. It is difficult
to maintain a small gap when polishing the surface of the workpiece. In order to prevent direct contact
between the workpiece and the polishing tool, a resin-coated polishing tool has been developed. In
this paper, a micro polishing tool was made using a plasma chemical vapor deposition method. The
geometry of the polishing tool was examined by a finite element method (FEM) to optimize the
concentration of the abrasive grains. In polishing machining using the tool, the width of the polishing
groove was 35 μm, and polishing machining in a micro area was achieved.
Publisher
Trans Tech Publications, Ltd.
Subject
Mechanical Engineering,Mechanics of Materials,General Materials Science
Cited by
5 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献