Abstract
Ti(C,N)-TiB2-WC composite ceramic cutting tool materials with nano-scale additives Ni and Mo, and micro-scale additives Ni and Mo as sintering aids were sintered respectively at a temperature of 1550 °C for holding time of 1hour in vacuum by a hot-press technique. The effects of nano-scale additives Ni and Mo, and micro-scale additives Ni and Mo on microstructure and mechanical properties of composites were compared and investigated. It is concluded that the wettability of nano-scale Ni and Mo to the composites is better than that of micro-scale Ni and Mo. The nano-scale whiskers were found in the composite ceramic tool materials with nano-scale additives. The addition of nano-scale Ni and Mo instead of micro-scale Ni and Mo could make the flexural strength and fracture toughness of Ti(C, N)-TiB2 –WC composites have a promotion, but could not make the hardness of the composites increase in this study.
Publisher
Trans Tech Publications, Ltd.
Subject
Mechanical Engineering,Mechanics of Materials,General Materials Science
Reference8 articles.
1. G.E. D'Errico, S. Bugliosi, E. Guglielmi: Mater. Proc. Tech. Vol. 77 (1998), p.337.
2. Sangho Park, Shinhoo Kang: Sci. Mater. Vol. 52 (2005), p.129.
3. H. Suzuki, K. Hayashi, H. Matsubara, K. Tokumoto: Powder. Metall. Vol. 30 (1983), p.106.
4. M. Ueki: Powder Metall. Vol. 40 (1993), p.743.
5. D. Mari, S. Bolognini, G. Feusier, T. Cutard, T. Viatte, W. Benoit: Int. J. Refract. Met. Hard Mater. Vol. 21 (2003), p.47~53.
Cited by
6 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献