Abstract
Sintering Behavior of Monolithic TiN and TiB2 Was Investigated Using Spark Plasma Sintering (SPS) at Temperatures between 1673 and 2573 K. Relative Density of TiN Was Increased from 82.3 to 96.7% while that of TiB2 Increased from 70.1 to 92.8% with Increasing Temperature. At Temperatures between 1673 and 2273 K, TiB2 Was More Difficult to Consolidate Compare to TiN. At 2473 K, TiB2 Densified Rapidly to 92.8%.
Publisher
Trans Tech Publications, Ltd.
Subject
Mechanical Engineering,Mechanics of Materials,General Materials Science
Cited by
2 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献
1. Combustion Synthesis of Eutectic TiB2/TiN Alloy;International Journal of Self-Propagating High-Temperature Synthesis;2019-01
2. TiN–TiB2 composites prepared by various sintering techniques;International Journal of Refractory Metals and Hard Materials;2013-11