The nano-TiO2powders with the average particle size of about 40nm were used as starting materials. The compacted powders were firstly performed in Spark-plasma-sintering (SPS) at a high temperature and then sintered in air for hours at a relatively low temperature. The obtained samples were investigated by X-ray diffraction (XRD) and scanning electron microscopy (SEM). The results showed an obvious reduction in grain size was achieved by taking advantage of modified two step sintering (MTSS). The value of the relative grain growth d/do for the samples prepared by MTSS was less than 3.
Publisher
Trans Tech Publications, Ltd.
Subject
Mechanical Engineering,Mechanics of Materials,General Materials Science
Reference10 articles.
1. H.G. KIM and K.T. KIM: Acta mater Vol. 47 (1999), p.3561.
2. Karel Maca, Vaclav Pouchly, Pavel Zalud: J. Eur. Ceram. Soc. Vol. 30 (2010), p.583.
3. S.C. Liao, Y.J. Chen, W. E. Mayo: Nanostruct. Mater. Vol. 11 (1999), p.553.
4. A . W eibel, R. Bouchet, R. Denoyel, P. Knauth: J. Eur. Ceram. Soc. Vol . 27 (2007), p.2641.
5. Jun Hong Noh, Hyun Suk Jung, Jung-Kun Lee, Jeong-Ryeol Kim: J. Eur. Ceram. Soc. Vol. 27 (2007), p.2937.