Abstract
In this paper, glass wool has been prepared under various rotating speed of centrifugal pan by centrifugal-spinneret-blow process. The fiber diameter of glass wool has been studied by scanning electron microscopy (SEM) and vertical optical microscope (VOM). With the increase of rotating speed from 1800 rpm to 2400 rpm, the mean fiber diameter decreased from 5.9 µm to 3.9 µm, indicating the distribution of glass wool becomes more uniformity. The results show that the rotating speed has a direct and pronounced effect on the fiber diameter and distribution. The higher the rotating speed is, the smaller the mean fiber diameter is, and the more uniformity the distribution of fiber diameter is.
Publisher
Trans Tech Publications, Ltd.
Reference7 articles.
1. S.M. Kirov, Obtaining glass fiber by a centrifugal-spinneret-blow method, Translated from Steklo i Keramika, 5 (1977) 16-18.
2. Markus Spinnler, Edgar Winter, Raymond Viskanta, Studies on high-temperature multilayer thermal insulations, International Journal of Heat and Mass Transfer, 47 (2004) 1305–1312.
3. Jing Chen, Masahiro Ueda, Katsuhiko Asada, et al., Realtime Densitometer for Glass Wool Using Solar Cells, Optics and Lasers in Engineering, 29 (1998) 61-66.
4. Standard of Performance for Wool Fiberglass Insulation Manufacturing Plants, 50 (1985) 7700.
5. Y.Z. Liu, Studies on process optimisation of multistage atomization, Materials Science and Technology, 18 (2002) 929-934.
Cited by
3 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献