Abstract
In the present study, various quantities of Bi2O3were added into 0.98(Na0.5Bi0.5)TiO3-0.02Ba(Sn0.08Ti0.92)O3(0.98NBT-0.02BST) ceramics. High-density samples were obtained through the addition of Bi2O3into 0.98NBT-0.02BST ceramic. It was found that 0.98NBT-0.02BST with the addition of 0~3.0 wt.% Bi2O3exhibit relatively good piezoelectric properties. For 0.98NBT-0.02BST ceramic with the addition of 2 wt.% Bi2O3, the electromechanical coupling coefficients of the planar mode kp and the thickness mode kt reach 0.12 and 0.61, respectively, at the sintering of 1100oC for 3 h. The ratio of thickness coupling coefficient to planar coupling coefficient is 5.1. It is obvious that 0.98NBT-0.02BST solid solution ceramic by adding low quantities of Bi2O3is one of the promising lead-free ceramics for high frequency electromechanical transducer applications.
Publisher
Trans Tech Publications, Ltd.
Reference26 articles.
1. T. Takenaka, K. Sakta and K. Toda: Ferroelectric Vol. 106 (1990), p.375.
2. T. Takenaka, K. Maruyama and K. Sakata: Jpn. J. Appl. Phys. Vol. 30 (1991), p.2236.
3. N. Ichinose, and K. Udagawa: Ferroelectric Vol. 169 (1995), p.317.
4. A. Sasa, T. Chiba, Y. Mamiya and E. Otsuki: Jpn. J. Appl. Phys. Vol. 38 (1999), p.5546.
5. C. H. Wang: J. Ceram. Soc. Jap. Vol. 116 [5] (2008), p.632.