Complex of properties of 2219 alloy weld joint in T62 state under modeling operating conditions

Author:

Nyrkova L.I.ORCID, ,Labur T.M.ORCID,Shevtsov E.I.,Nazarenko O.P.,Dorofeev A.V.,Osadchuk S.O.ORCID,Yavorska M.R.ORCID,Poklyatsky A.G.ORCID,Fedorchuk V.E.ORCID, , , , , , , ,

Abstract

A complex of properties of aluminium alloy 2219 welded joint, made by single-pass welding with a non-fusible electrode along and across the rolled product, and heat-treated to the state T62, in liquid amyl and its vapors at a temperature of 50 °C for 45 days was investigated. Characteristics of plasticity and strength of 2219 alloy welded joints are as follows: in the longitudinal (D) direction – yield strength of the welded joint is (301–317) MPa, of the base metal (295—297) MPa, strength limit of the welded joint (409–415) MPa, of the base metal (422–425) MPa, elongation is (4.0–5.8)% and (17.6–19.1)%, respectively; in the transverse (P) direction – the yield strength of the welded joint is (309–331) MPa, of the base metal (304–307) MPa, the yield strength of the welded joint (392–414) MPa, of the base metal (428–433) MPa, elongation is (2.1–3.3)% and (12.6–15.0)%, respectively. The strength coefficient of welded joints in the longitudinal direction is 0.96, in the transverse – 0.94. Welded joints in the above environment are resistant to corrosion cracking and intergranular corrosion, resistance against exfoliating corrosion is evaluated by grade 2. Resistance of 2219 alloy in T62 state in amyl corresponds to the resistance group «stable», in amyl vapors – the group “highly resistant”. After aging in amyl and amyl vapors, the strength grades of the base metal samples and welded joints in both directions are almost unchanged, the plasticity parameters change ambiguously: the yield strength of the base metal increases by ~ (5–6)%, of welded joints decreases by ~ (6–7)%, the relative elongation of the base metal is reduced by ~ (5–16)%, of welded joints by about ~ 20 %. Independently of the direction of welding relative to metal’s rolling, samples’ fractures are mostly viscous. After the exposing in amyl, the coefficient of the strength of welded joints in the longitudinal and transverse directions is the same and equal to 0.91, after the influence of amyl vapors, it is 0.95 in the longitudinal direction and 0.96 in the transverse direction.

Publisher

National Academy of Sciences of Ukraine (Co. LTD Ukrinformnauka) (Publications)

Subject

Anesthesiology and Pain Medicine

Reference40 articles.

1. 1. John E. Hatch. (1989). Aluminum: Properties and Physical Metallurgy: A Handbook. Per. from English. Publisher: Metallurgy [in Russian].

2. 2. АМS-QQ-А-250/30А. Technical requirements. Aluminum alloy 2219. Sheet and plate.

3. 3. GOST 7512-82 Nondestructive testing. Welded joints. Radiography method, Moscow, Izd-vo standartov [in Russian].

4. 4. GOST 9.904-82 Unified system of corrosion and ageing protection. Alluminium alloys. Accelerated test method for exfoliating corrosion, Moscow, Izd-vo standartov [in Russian].

5. 5. GOST 9.021-74 Unified system of corrosion and ageing protection. Aluminium and aluminium alloys. Accelerated test

Cited by 4 articles. 订阅此论文施引文献 订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献

同舟云学术

1.学者识别学者识别

2.学术分析学术分析

3.人才评估人才评估

"同舟云学术"是以全球学者为主线,采集、加工和组织学术论文而形成的新型学术文献查询和分析系统,可以对全球学者进行文献检索和人才价值评估。用户可以通过关注某些学科领域的顶尖人物而持续追踪该领域的学科进展和研究前沿。经过近期的数据扩容,当前同舟云学术共收录了国内外主流学术期刊6万余种,收集的期刊论文及会议论文总量共计约1.5亿篇,并以每天添加12000余篇中外论文的速度递增。我们也可以为用户提供个性化、定制化的学者数据。欢迎来电咨询!咨询电话:010-8811{复制后删除}0370

www.globalauthorid.com

TOP

Copyright © 2019-2024 北京同舟云网络信息技术有限公司
京公网安备11010802033243号  京ICP备18003416号-3