Affiliation:
1. Department of Pediatric Dentistry and Orthodontics, Peoples’ Friendship University of Russia, Moscow, Russia
Abstract
This study aimed to investigate the effect of final sintering on the thermal properties and phase composition of yttrium-stabilized zirconium dioxide.
Totally 15 yttrium-stabilized zirconium oxide standard ovoid samples were studied (3Y-TZP, IPS e.max ZirCAD LT, Ivoclar Vivadent, Schaan, Liechtenstein). This material contains the following components: ZrO2 - 87.0 - 95.0%, Y2O3 - 4.0 - 6.0%, HfO2 - 1.0 - 5.0%, Al2O3 - 0.0 - 1, 0%. Initially, X-ray diffraction analysis was performed. After that, differential scanning calorimetry was carried out up to a temperature of 900°C. X-ray diffraction analysis was performed to assess the effect of the firing process on the phase analysis of zirconia samples (Selected samples were tested on an X-ray diffraction instrument (EMPYREAN, PANalytical, Lelyweg, The Netherlands) The thermal changes study in zirconia samples resulting from repetitive firing processes was performed then. Samples were placed in a differential scanning calorimeter (NETZSCH STA 409 PC Luxx, Bavaria, Germany) and heated at a rate of 10°C/min from 50°C to 900°C.) Then, differential scanning calorimetry data (the mass and structural changes of zirconia samples depending on temperature) was recorded.
The percentage of the monoclinic phase increases on average from 3.6% to 7.5%, but this difference is not statistically significant (p=0.1). Two exothermic peaks were observed when the samples were heated from 50°C to 900°C.
The final firing of 3Y-TZP zirconium crown up to 900°C slightly increases the content of the monoclinic phase and causes exothermal changes.
Publisher