A Study of Factors Responsible for Cracking during Drying of Thick Aqueous-Processed NMC811 Cathodes

Author:

Sahore RituORCID,Li Jianlin,Wood David L.

Abstract

Replacing the widely used NMP solvent for processing of lithium-ion battery electrodes with water has both environmental and cost benefits. Compared to aqueous-processing of anodes, the aqueous-processing of cathodes is considerably more challenging. Issues such as damage of the NMC-type active material upon exposure to water, damage of the aluminum substrate due to highly basic aqueous-slurry, and cracking of the water-based cathode slurry coatings upon drying are known and are actively being researched. In this study, we focus on the cracking-issue which is more severe for relatively thick cathodes with loadings of >~11-12 mg/cm2. Our group has previously reported the role of high surface-tension of water compared to NMP on cracking and demonstrated that the addition of 20-30 wt% IPA as a co-solvent lead to crack-free thick (~25 mg/cm2) NMC532 cathodes. This finding was attributed to reduction of surface tension of water, which decreased the capillary forces during drying. Further investigations have resulted in identification of several other factors that are also responsible for the cracking-issue. These factors, which are not necessarily related to the surface tension, will be discussed.

Publisher

The Electrochemical Society

Cited by 3 articles. 订阅此论文施引文献 订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献

同舟云学术

1.学者识别学者识别

2.学术分析学术分析

3.人才评估人才评估

"同舟云学术"是以全球学者为主线,采集、加工和组织学术论文而形成的新型学术文献查询和分析系统,可以对全球学者进行文献检索和人才价值评估。用户可以通过关注某些学科领域的顶尖人物而持续追踪该领域的学科进展和研究前沿。经过近期的数据扩容,当前同舟云学术共收录了国内外主流学术期刊6万余种,收集的期刊论文及会议论文总量共计约1.5亿篇,并以每天添加12000余篇中外论文的速度递增。我们也可以为用户提供个性化、定制化的学者数据。欢迎来电咨询!咨询电话:010-8811{复制后删除}0370

www.globalauthorid.com

TOP

Copyright © 2019-2024 北京同舟云网络信息技术有限公司
京公网安备11010802033243号  京ICP备18003416号-3