The galvanic corrosion of the β-phase (Al3Mg2)/Al couple has been studied using electrochemical methods, scanning vibrating electrode technique (SVET) and Time of flight-secondary ion spectroscopy (ToF-SIMS). Polarization tests reveal that Al3Mg2 is anodic relative to pure Al at pH ≤ 10. Visualization of the current density distribution over the Al3Mg2/Al galvanic couple by SVET reveals that at pH 2, an intense and stochastic anodic current density is evolved from Al3Mg2 while a heavy cathodic current flux is sustained on the surrounding Al matrix. At pH 6 and 10, localized both cathodic and anodic regions are seen on Al3Mg2 indicating its self-dissolution while the surrounding Al matrix remained relatively inert. However, at pH 13, a reversal of polarity occurs and Al3Mg2 becomes cathodic relative to Al. The severity of the galvanic coupling of Al3Mg2 to Al is in the order pH 13 > pH 2 > pH 6 > pH 10. ToF-SIMS analysis reveals that the dealloying of Al3Mg2 in the galvanic couple is by selective dissolution of Mg leading to the deposition of corrosion products dominated by Mg compounds in an acidic and neutral environment. In an alkaline environment, a relatively thin hydroxide rich film is formed.
Funder
National Natural Science Foundation of China
Publisher
The Electrochemical Society
Subject
Materials Chemistry,Electrochemistry,Surfaces, Coatings and Films,Condensed Matter Physics,Renewable Energy, Sustainability and the Environment,Electronic, Optical and Magnetic Materials
Cited by
27 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献