Abstract
The paper focuses on the analysis of initiation and propagation of CO2 corrosion in several samples of low-alloy steel with different microstructures using scanning electrochemical microscopy (SECM) and other microscopy techniques. It is found that the corrosion rate and the mode of corrosion are highly sensitive to the microstructure. The overall current density is much higher and more uniformly distributed for the tempered martensite structure than for samples having either a ferritic-pearlitic microstructure or a microstructure combining ferritic, bainitic and martensitic-austenitic regions. As a result, the sample with the tempered martensite structure undergoes uniform corrosion, while the other two samples undergo selective corrosion. The SECM maps show that regions of polygonal ferrite generate larger anodic currents than the pearlitic structure in the early stages of corrosion. The residual cementite provides greater cathodic surface areas after the initial dissolution of ferritic lamellae within pearlite, promoting galvanic corrosion and subsequently enhanced dissolution of ferritic lamellae. According to SECM data, the dissolution of iron in polygonal ferritic grains is 2.4 times faster than that of ferritic lamellae in pearlitic regions.
Funder
Danish offshore Technology Centre
Publisher
The Electrochemical Society
Subject
Materials Chemistry,Electrochemistry,Surfaces, Coatings and Films,Condensed Matter Physics,Renewable Energy, Sustainability and the Environment,Electronic, Optical and Magnetic Materials
Cited by
8 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献