Abstract
An experimental protocol is developed to measure the shear strength of NMC811 single crystals within the cathode of a lithium-ion cell. The cathode is placed upon a set of thick metallic substrates that possess a wide range of indentation hardness. For each choice of substrate, the top surface of the cathode is indented by a Vickers indenter to a sufficient depth that the cathode layer is subjected to an approximately spatially uniform compressive normal traction equal to the hardness of the substrate. The sensitivity of plastic flow and fracture of the single crystals to substrate hardness is determined by observation of the particles in the indented top surface of the cathode using a scanning electron microscope. It is found that the shear strength of fully lithiated NMC811 single crystals along their basal plane is 86 ± 12 MPa, and decreases to 39 ± 5 MPa upon cell charging (delithiation of the cathode). This implies that particle slip and fracture will occur under mild mechanical loading, for example by calendering during manufacture and by electrical cycling of the compacted cathode. The indentation protocol developed here has application to a wide range of single crystal cathode materials.
Funder
Faraday Institution
H2020 European Research Council
Publisher
The Electrochemical Society
Subject
Materials Chemistry,Electrochemistry,Surfaces, Coatings and Films,Condensed Matter Physics,Renewable Energy, Sustainability and the Environment,Electronic, Optical and Magnetic Materials
Cited by
15 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献