AbstractAssessing the risk of cracking of high performance concrete induced by restrained volume changes from early ages is of considerable significance. To estimate and control such cracking risk of high performance concrete, two characteristic temperatures, namely zero-stress temperature (Tz) and cracking temperature (Tx) are crucial. In this study, the two temperatures are investigated in-depth by both theoretical analysis and experimental studies. For predicting the evolutions of Tz and Tx from early ages, rigorous yet practical models are proposed, which crucially take the visco-elastic behaviour of concrete into account. The reliability and predictive capability of the proposed models are demonstrated through a series of comparisons between the predicted and the measured results. Based on the predicted Tz and Tx profiles, practical thermal control criteria for preventing concrete from cracking caused by restrained strain are put forward. In principle, the actual temperature (T) of concrete should be kept higher than both Tz and Tx to properly maintain the stress induced by restrained strain in compression at early ages. If T becomes lower than Tz and reduces continuously, the lower the value of T, the higher the risk of cracking of concrete induced by restrained strain. As a consequence, once the value of T reaches or becomes lower than Tx, cracking is highly likely to occur. For a given actual temperature condition, lowering Tz and Tx can mitigate the risk of the cracking of concrete. Finally, effective measures for such lowering of Tz and Tx are also proposed.
Funder
Australian Research Council
The University of Queensland
Publisher
Springer Science and Business Media LLC
Subject
Mechanics of Materials,General Materials Science,Building and Construction,Civil and Structural Engineering
Reference48 articles.
1. Benboudjema F, Carette J, Delsaute B et al (2018) Chapter 4 mechanical properties. In: Fairbairn EMR, Azenha M (eds) Thermal cracking of massive concrete structures: state of the art report of the RILEM Technical Committee 254-CMS. Springer, Berlin, pp 69–114
2. Mechtcherine V, Gorges M, Schroefl C et al (2014) Effect of internal curing by using superabsorbent polymers (SAP) on autogenous shrinkage and other properties of a high-performance fine-grained concrete: Results of a RILEM round-robin test. Mater Struct 47:541–562. https://doi.org/10.1617/s11527-013-0078-5
3. Jensen OM, Lura P (2006) Techniques and materials for internal water curing of concrete. Mater Struct 39:817–825. https://doi.org/10.1617/s11527-006-9136-6
4. Cusson D, Hoogeveen T (2008) Internal curing of high-performance concrete with pre-soaked fine lightweight aggregate for prevention of autogenous shrinkage cracking. Cem Concr Res 38:757–765. https://doi.org/10.1016/j.cemconres.2008.02.001
5. Li L, Dabarera AGP, Dao V (2020) Time-zero and deformational characteristics of high performance concrete with and without superabsorbent polymers at early ages. Constr Build Mater 264:120262. https://doi.org/10.1016/j.conbuildmat.2020.120262
Cited by
3 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献