Kar B.,Sahoo H.,Rath S. S.,Rao D. S.,Das B.
Abstract
AbstractA china clay sample from Jharkhand State, India, containing 65.0 wt.% SiO2, 22.7% Al2O3, 1.77% Fe2O3and 9.10% LOI was subjected to physical beneficiation and acid leaching studies to improve its quality. The clay was characterized by optical microscopy, XRD, and wet chemical analysis methods. Quartz and goethite are the two major impurities. High intensity magnetic separation removed only 10% of the total iron. Experiments with oxalic acid were carried out to establish the leaching kinetics of iron and the effects of acid concentration, time and temperature on iron leaching were also examined. The study demonstrated that ∼90% of total iron could be removed using 5% oxalic acid. The dissolution of iron from clay is best described by diffusion of ions through the product layer of constant size spherical particles. The activation energy of the leaching process over the temperature range was calculated to be 51.14 kJ/mol.
Subject
Geochemistry and Petrology
Cited by
8 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献