1. 1) B.V. Reddy and S.C. Deevi: "Thermophysical properties of FeAl (Fe-40 at.% Al)", Intermetallics, 8 (2000) 1369-1376.
2. 2) U. Reimann1 and G. Sauthoff: "Efects of deviations from stoichiometry on the deformation behaviour of FeAl at intermediate temperatures", Intermetallics, 7 (1999) 437-445.
3. 3) C.T. Liu, E.P. George, P.J. Maziasz, and J.H. Schneibel: "Recent advances in B2 iron aluminide alloys: deformation, fracture and alloy design", Mater. Scie. Eng. A, A258 (1998) 84-98.
4. 4) Y. Terada, K. Ohkubo, K. Nakagawa, T. Mohri, and T. Suzuki: "Thermal conductivity of B2-type aluminides and titanides", Intermetallics, 3 (1995) 347-355.
5. 5) K. Katou, A. Matsumoto, S. Zheng Ming, K. Shimojima, H. Hosokawa, M. Takada, and T. Hiramatsu: "Preparation for WC-FeAl hard metal by vacuum sintering", J. Jpn. Soc. Powder Powder Metallurgy, 58 (2011) 500-505.