1. 1) Japanese Standards Association; JIS G3129: 2005 High Tensile Strength Steel for Tower Structural Purposes.
2. 2) T. Takeda; Evaluation Method of Zinc Induced Cracking, Quarterly Journal of The Japan Welding Society 71-4 (2002), 32-38. (in Japanese)
3. 3) T. Takeda, K. kanaya, K. Yamato, K. Eiro, Z. Chano, S. Kanazawa, T. Hiroki and T. Iezawa; Development of 60Kgf/mm2 Steel for Power-transmission Pipe Tower and Its Resistance to Liquid Zinc Embrittlement, Transactions of the Iron and Steel Institute of Japan (1984), 124-130. (in Japanese)
4. 4) Y. Miyauchi, G. Etoh, K. Funami, H. Shimizu and H. Yasui; Effect of Hot Dip Galvanizing on Strength of 60Kgf/mm2 Class Tensile Strength Steel, Transactions of the Japan Society of Mechanical Engineers N0.932-1, P.67-69, 1993. (in Japanese)
5. 5) K. Kanaya, T. iezawa, S. Kanazawa and Y. Ishida; Penetration Behavior of Zn along Prior γ Grain Boundary during Galvanizing of Steel Structures, Tomoe Corporation Technical Report No.10 P.67-75. (in Japanese)