1. 7) T.Inoue, T.Ishikawa, S.Imai, T.Koseki, K.Hirota, M.Tada, H.Kitada, Y.Yamaguchi, H.Yajima, Long crack arrestability of heavy-thick shipbuilding steels, Proc. 16th Int. Offshore and Polar Engineering Conf., San Francisco, 2006, 132-136.
2. 13) Y.Yamaguchi, H.Yajima, S.Aihara, H.Yoshinari, K.Hirota, M.Toyoda, T.Kiyose, S.Tanaka, T.Okabe, K.Kakegama, Y.Funatsu, T,Handa, T.Kawabata, T.Tani, Development of guidelines on brittle crack arrest design, Proc. 20th Int. Offshore and Polar Engineering Conf., Beijing, 2010, 71-79.
3. 15) F.J.Feely, M.S.Northup, S.R.Kleep, M.Gensamer, Studies on the brittle failure of tanlkage steel plate, Welding Jounrnal, 34, 1955, pp.596s-607s.
4. 16) D.J.Naus, J.Keeney-Walker, B.R.Bass, R.J.Fields, R.deWit, S.R.Low III, High-temperature crack-arrest behavior of prototypical and degraded reactor pressure vessel steels, Int. J. Pressure Vessels and Pipings, 39 (1989), pp.189-208.
5. 18) T.Kawabata, K.Matsumoto, T.Ando, H.Yajima, S.Aihara, H.Yoshinari, K.Hirota, M.Toyoda, T.Kiyose, T.Inoue, T.Handa, T.Tani, Development of brittle crack arrest toughness Kca test method, Proc. 20th Int. Offshore and Polar Engineering Conf., Beijing, 2010, 80-87.