AbstractPolymers are omnipresent in our everyday lives. For specific applications, their properties can be extensively modified by various types of additives, e.g., processing stabilizers, antioxidants, UV-stabilizers, flame retardants, and plasticizers. While several additives are nowadays considered to be toxic or persistent in the environment, quantitative data characterizing plastic fragmentation and microplastic formation have not yet been discussed in detail. Here, we present a long-term, laboratory-controlled accelerated weathering study on polypropylene (PP) particles with and without processing stabilizers. We were able to identify the stabilizers as Irgafos® 168, and Irganox® 1010. For both PP sample sets, we monitored the degradation using a combination of various analytical methods, such as gel permeation chromatography, particle size distributions, scanning electron microscopy, solid-state 13C magic-angle spinning NMR and liquid-state 1H, 13C, 31P NMR spectroscopy, differential scanning calorimetry and matrix-assisted laser desorption ionization time of flight mass spectrometry. The stabilizers prevent degradation by simulated solar radiation for about 350 h. Then, degradation sets in rapidly, leading to an exponential decrease in molecular weight and particle size, accompanied by an increase in crystallinity and the formation of oxygen-containing functional groups. After 3200 h, representing approximately 2 years of outdoor weathering, both PP samples exhibit comparable characteristics and sizes, regardless if a stabilizer was initially present. During degradation, an extremely large number of 100,000 daughter particles (4 µm) are formed and released from one MP particle of 192 µm diameter. Their physical properties and chemical composition have largely changed, resulting in a very low molecular weight and a hydrophilic character. These particles no longer resemble pristine PP. We thus expect them to be more prone to biodegradation compared to the starting material.

Funder

Universität Bayreuth

Publisher

Springer Science and Business Media LLC

Subject

Environmental Engineering

同舟云学术

1.学者识别学者识别

2.学术分析学术分析

3.人才评估人才评估

"同舟云学术"是以全球学者为主线,采集、加工和组织学术论文而形成的新型学术文献查询和分析系统,可以对全球学者进行文献检索和人才价值评估。用户可以通过关注某些学科领域的顶尖人物而持续追踪该领域的学科进展和研究前沿。经过近期的数据扩容,当前同舟云学术共收录了国内外主流学术期刊6万余种,收集的期刊论文及会议论文总量共计约1.5亿篇,并以每天添加12000余篇中外论文的速度递增。我们也可以为用户提供个性化、定制化的学者数据。欢迎来电咨询!咨询电话:010-8811{复制后删除}0370

www.globalauthorid.com

TOP

Copyright © 2019-2024 北京同舟云网络信息技术有限公司
京公网安备11010802033243号  京ICP备18003416号-3