Abstract
AbstractAmorphous silicon-nitride thin films a-Si:N:H were obtained by plasma enhanced chemical vapour deposition (PECVD) method from SiH4+NH3 at 13.56 MHz. The process parameters were chosen to obtain the films of properties suitable for optoelectronic and mechanical applications. FTIR analysis of a-Si:N:H films indicated the presence of numerous hydrogen bonds (Si-H and N-H) which passivate structural defects in multicrystalline silicon and react with impurities. The morpho-logical investigations show that the films are homogeneous. The deposition of a-Si:N:H layers leads to the decrease in friction coefficient of used substrates. Optical properties were optimised to obtain the films of low effective reflectivity, large energy gap Eg from 2.4 to 2.9 eV and refractive index in the range of 1.9 to 2.2. Reduction of friction coefficient for monocrystalline silicon after covering with a-Si:N:H films was observed: from 0.25 to 0.18 for 500 cycles.
Subject
Electrical and Electronic Engineering,Radiation,General Materials Science
Reference15 articles.
1. Determination of the thickness and optical constants of amorphous silicon;Swanepol;Phys Sci Instrum,1983
2. Amorphous hydrogenated silicon nitride films for applications in solar cells;Swatowska;Vacuum,2008
3. PC Version bit so lar cell modelling on personal computers Record of the th IEEE Photovoltaic Specialists;Clugston;Conf,1997
4. Optical structural and electrical properties of device quality a Si films grown by plasma enhanced chemical vapour de position;Giorgis;Phil Mag,1998
5. Phosphorus diffused silicon solar cell emitters with plasma enhanced chemical vapour depo sited silicon carbide;Orpella;Energ Mat Sol,2005
Cited by
7 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献