1. Zhelobtsov, E.A., Isakaev, E.Kh., Peletskii, V.E., and Tyuftyaev, A.S., Instrum. Exp. Tech., 2009, vol. 52, no. 5, p. 743.
2. Maglic, K.D., Cezairliyan, A., and Peletsky, V.E., Compendium of Thermophysical Property Measurement Methods: Volume 2. Recommended Measurement Techniques and Practices, New York: Plenum, 1992, p. 133.
3. Oleinik, B.N., Sokolov, N.A., and Raskin, A.A., Stal’ nerzhaveyushchaya marki 12Kh18N10T. Teploprovodnost’ pri temperaturakh 340–1100 K. Tablitsy standartnykh spravochnykh dannykh 1 GSSSD 165-94 (State Service of Standard Reference Data 165-94. Stainless Steel 12Kx18N10T: Thermal Conductivity at Temperatures in the Range from 340 to 1100 K), Moscow: Izd. Standartov, 1994.
4. Lykov, A.M., Fiz. Khim. Obrab. Mater., 2008, no. 2, p. 71.
5. Samotugin, S.S., Mazur, V.A., and Litvinenko, D.S., Visn. SevNTU, Ser.: Mashinopriladobuduvannya Transp., 2012, no. 129, p. 195.