1. A. M. Bol’shakov, “Cold resistance of pipelines and tanks in the North after long-term operation,” Tyazh. Mashinostr., No. 8, 20–25 (2010).
2. A. S. Syromyatnikova, “Degradation of the physicomechanical state of the gas main pipe metal during long-term operation under cryolite conditions,” Fiz. Mezomekh., No. 17, 85–91 (2014).
3. O. I. Sleptsov, A. M. Bol’shakov, A. V. Lyglaev, and L. N. Tatarinov, “Structure and properties of the gas main pipe metal after operation for 30 years under extreme north conditions,” Deform. Razr. Mater., No. 3, 21–23 (2006).
4. A. A. Gilyazov, A. M. Bol’shakov, N. I. Golikov, A. A. Alekseev, S. A. Sintsov, R. P. Tikhonov, A. R. Ivanov, and L. N. Tatrinov, “Carrying capacity of aging gas mains under extreme north conditions,” Gazov. Prom., No. 1, 38–39 (2006).
5. A. A. Alekseev, A. S. Syromyatnikova, A. M. Bol’shakov, and A. R. Ivanov, “Catastrophic fracture of pipelines and tanks with crack branching,” Bezop. Truda Promysh., No. 1, 42–44 (2013).