1. Serebryakova, T.I., Neronov, V.A., and Peshev, P.D., Vysokotemperaturnye boridy (High-Temperature Borides), Moscow: Metallurgiya, 1991.
2. Ibrahiem, M.O., Foosnes, T., and Oye, H.A., Properties of pitch and furan-based TiB2–C cathodes, Light Metals: 2008 TMS Annual Meeting, New Orleans, 2008, vol. 4, pp. 1013–1018.
3. Li, J., Lu, X.-j., Lai, Y.-q., Li, Q.-y., and Liu, Y-x., Research progress in TiB2 wettable cathode for aluminum reduction, JOM, 2008, no. 8, pp. 32–37.
4. Ivanov, V.V., Kirik, S.D., Shubin, A.A., Blokhina, I.A., Denisov, V.M., and Irtugo, L.A., Thermolysis of acidic aluminum chloride solution and its products, Ceram. Int., 2013, vol. 39, pp. 3843–3848.
5. Ma Ai-dong and Jiang Ming-xue, The Thermodynamic Analysis on the system of TiO2–B2O3—C, Bull. Chin. Ceram. Soc., 2008, vol. 27, no. 5, pp. 957–962.