1. A. V. Ioffe, “Fracture mechanism of tube steels in sulfur-bearing medium,” Candidate’s Dissertation in Engineering (Tolyatty, 2000).
2. Corrosion-Active Nonmetallic Inclusions in Carbon and Low-Alloyed Steels, Ed. by I. G. Rodionova, A. I. Zaitsev, and O. N. Baklanova (Metallurgizdat, Moscow, 2005).
3. Yu. P. Surkov, O. M. Sokolova, V. G. Rybalko, and L. F. Malkova, “Diagnostics of industrial fractures. An analysis of fracture factors and the mechanisms of defectiveness of main pipeline from 17GS steel,” Fiz.–Khim. Mekh. Mater., No. 5, 95–97 (1989).
4. T. K. Sergeeva, N. I. Volgina, M. V. Ilyukhina, and A. S. Bolotov, “Corrosion cracking of gas-duct tubes in weakly-acid soil,” Gazovaya Promyshlennosn’, No. 4, 34–38 (1995).
5. A. V. Dub, N. V. Barulenkova, T. V. Morozova, S. V. Efimov, V. N. Filatov, S. D. Zinchenko, and A. M. Lamukhin, “Nonmetallic inclusions in lowalloyed tube steel,” Metallurg, No. 4, 67–73 (2004).