Comparison of Shear Strength of Metal and Ceramic Orthodontic Brackets Cemented to Zirconia Depending on Surface Treatment: An In Vitro Study

Author:

Cetik Sibel1ORCID,Ha Thaï Hoang2,Sitri Léa2,Duterme Hadrien2,Pham Viet2,Atash Ramin3

Affiliation:

1. Department of Stomatology and Dentistry, Erasmus Hospital and Laboratory of Physiology and Pharmaceutics, Faculty of Medicine, Université Libre de Bruxelles, Brussels, Belgium

2. Department of Stomatology and Dentistry, Erasmus Hospital, Université Libre de Bruxelles, Brussels, Belgium

3. Dental Materials Research Center, School of Dentistry, Isfahan University of Medical Sciences, Isfahan, Iran and Department of Stomatology and Dentistry, Erasmus Hospital, Université Libre de Bruxelles, Brussels, Belgium

Abstract

Abstract Objectives Due to the high demand for all-ceramic restorations, monolithic zirconia restorations are nowadays frequently used. With the demand for adult orthodontic treatments, orthodontists need to be mindful of the quality of their brackets bonding to this type of material, as it requires special conditioning. This study aimed to compare different surface treatments of zirconia when bonding metal or ceramic orthodontic brackets. The objectives are to compare the shear bond strength; the amount of adhesive remaining on the surface of the material; the incidence of adhesive, cohesive, and mixed failures; and the occurrence of zirconia fractures. Materials and Methods Forty monolithic blocks of zirconia of a diameter of 10 mm and a length of 10 mm were prepared and randomly divided into two groups (n = 20): metallic or ceramic brackets. Each group was subsequently divided into two subgroups (n = 10) depending on the surface preparation (laser treatment or airborne particle abrasion): SMB (airborne particle abrasion, metal bracket), SCB (airborne particle abrasion, ceramic bracket), LMB (laser; metal bracket), and LCB (laser, ceramic bracket). The samples were tested for shear bond strength using a universal testing machine. The adhesive remnant index and the occurrence of zirconia fractures and different types of failures were assessed by optical and electron microscopy. Statistical Analysis Results were analyzed using analysis of variance. Results The differences were significant between the metallic (SMB, LMB) and ceramic (SCB, LCB) bracket groups with regard to shear bond strength, with respectively 23.29 ± 5.34 MPa, 21.59 ± 4.03 MPa, 20.06 ± 4.05 MPa, and 17.55 ± 3.88 MPa. In terms of surface treatment, no statistical differences were found between the different groups. Conclusion Metal brackets have a greater bond strength than ceramic brackets when cemented to zirconia. The surface treatment of zirconia surface has no influence on the shear bond strength.

Publisher

Georg Thieme Verlag KG

Subject

General Dentistry

同舟云学术

1.学者识别学者识别

2.学术分析学术分析

3.人才评估人才评估

"同舟云学术"是以全球学者为主线,采集、加工和组织学术论文而形成的新型学术文献查询和分析系统,可以对全球学者进行文献检索和人才价值评估。用户可以通过关注某些学科领域的顶尖人物而持续追踪该领域的学科进展和研究前沿。经过近期的数据扩容,当前同舟云学术共收录了国内外主流学术期刊6万余种,收集的期刊论文及会议论文总量共计约1.5亿篇,并以每天添加12000余篇中外论文的速度递增。我们也可以为用户提供个性化、定制化的学者数据。欢迎来电咨询!咨询电话:010-8811{复制后删除}0370

www.globalauthorid.com

TOP

Copyright © 2019-2024 北京同舟云网络信息技术有限公司
京公网安备11010802033243号  京ICP备18003416号-3