Author:
Hebbale Ajit M.,Kumar Manish,Soudagar Manzoore Elahi Mohammad,Ahamad Tansir,Kalam Md. Abul,Mubarak Nabisab Mujawar,Alfantazi Akram,Khalid Mohammad
Abstract
AbstractA typical ferrite/martensitic heat-resistant steel (T91) is widely used in reheaters, superheaters and power stations. Cr3C2-NiCr-based composite coatings are known for wear-resistant coatings at elevated temperature applications. The current work compares the microstructural studies of 75 wt% Cr3C2- 25 wt% NiCr-based composite clads developed through laser and microwave energy on a T91 steel substrate. The developed clads of both processes were characterized through a field emission scanning electron microscope (FE-SEM) attached with energy-dispersive X-ray spectroscopy (EDS), X-ray diffraction (XRD) and assessment of Vickers microhardness. The Cr3C2-NiCr based clads of both processes revealed better metallurgical bonding with the chosen substrate. The microstructure of the developed laser clad shows a distinctive dense solidified structure, with a rich Ni phase occupying interdendritic spaces. In the case of microwave clad, the hard chromium carbide particles consistently dispersed within the soft nickel matrix. EDS study evidenced that the cell boundaries are lined with chromium where Fe and Ni were found inside the cells. The X-ray phase analysis of both the processes evidenced the common presence of phases like chromium carbides (Cr7C3, Cr3C2, Cr23C6), Iron Nickel (FeNi3) and chromium-nickel (Cr3Ni2, CrNi), despite these phases iron carbides (Fe7C3) are observed in the developed microwave clads. The homogeneous distributions of such carbides in the developed clad structure of both processes indicated higher hardness. The typical microhardness of the laser-clad (1142 ± 65HV) was about 22% higher than the microwave clad (940 ± 42 HV). Using a ball-on-plate test, the study analyzed microwave and laser-clad samples' wear behavior. Laser-cladding samples showed superior wear resistance due to hard carbide elements. At the same time, microwave-clad samples experienced more surface damage and material loss due to micro-cutting, loosening, and fatigue-induced fracture.
Publisher
Springer Science and Business Media LLC
Reference42 articles.
1. Yang, G. J., Li, C. J., Zhang, S. J. & Li, C. X. High-temperature erosion of HVOF sprayed Cr 3C 2-NiCr coating and mild steel for boiler tubes. J. Therm. Spray Technol. 17(5–6), 782–787 (2008).
2. Wu, H. & Kong, D. Effects of laser power on friction–wear performances of laser thermal sprayed Cr3C2–NiCr composite coatings at elevated temperatures. Opt. Laser Technol. 117, 227–238 (2019).
3. Hebbale, A. M. & Srinath, M. S. Microstructural investigation of Ni based cladding developed on austenitic SS-304 through microwave irradiation. J. Mater. Res. Technol. 5(4), 293–301 (2016).
4. Singh, H., Kaur, M. & Prakash, S. High-temperature exposure studies of HVOF-sprayed Cr3C2-25(NiCr)/(WC-Co) coating. J. Therm. Spray Technol. 25(6), 1192–1207 (2016).
5. Janka, L., Norpoth, J., Eicher, S., Rodríguez, M. & Vuoristo, P. Improving the toughness of thermally sprayed Cr 3 C 2 -NiCr hardmetal coatings by laser post-treatment. JMADE 98, 135–142 (2016).
Cited by
2 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献