Comparative study of eco-friendly wire mesh configurations to enhance sustainability in reinforced concrete structures

Author:

Mebrahtom Misgina,Fissha Yewuhalashet,Ali Mujahid,Gebretsadik Angesom,Kide Yemane,Nguse Zaid,Gebrehiwot Zemicael,Flores Erick Saavedra,Avudaiappan Siva,Ikeda Hajime

Abstract

AbstractRecent and past studies mainly focus on reducing the dead weight of structure; therefore, they considered lightweight aggregate concrete (LWAC) which reduces the dead weight but also affects the strength parameters. Therefore, the current study aims to use varied steel wire meshes to investigate the effects of LWAC on mechanical properties. Three types of steel wire mesh are used such as hexagonal (chicken), welded square, and expanded metal mesh, in various layers and orientations in LWAC. Numerous mechanical characteristics were examined, including energy absorption (EA), compressive strength (CS), and flexural strength (FS). A total of ninety prisms and thirty-three cubes were made. For the FS test, forty-five 100 × 100 × 500 mm prism samples were poured, thirty-three 150 × 150 × 150 mm cube samples were made, and forty-five 400 × 300 × 75 mm EA specimens were costed for fourteen days of curing. The experimental findings demonstrate that the FS was enhanced by adding additional forces that spread the forces over the section. One layer of chicken, welded, and expanded metal mesh enhances the FS by 52.96%, 23.76%, and 22.2%, respectively. In comparison to the remaining layers, the FS in a single-layer hexagonal wire mesh has the maximum strength, 29.49 MPa. The hexagonal wire mesh with a single layer had the greatest CS, measuring 36.56 MPa. When all three types of meshes are combined, the CS does not vary in this way and is estimated to be 29.79 MPa. In the combination of three layers, the chicken and expanded wire mesh had the most energy recorded prior to final failure, which was 1425.6 and 1108.7 J, whereas it was found the highest 752.3 J for welded square wire mesh. The energy absorption for the first layer with hexagonal wire mesh increased by 82.81% prior to the crack and by 88.34% prior to the ultimate failure. Overall, it was determined and suggested that hexagonal wire mesh works better than expanded and welded wire meshes.

Publisher

Springer Science and Business Media LLC

Cited by 1 articles. 订阅此论文施引文献 订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献

同舟云学术

1.学者识别学者识别

2.学术分析学术分析

3.人才评估人才评估

"同舟云学术"是以全球学者为主线,采集、加工和组织学术论文而形成的新型学术文献查询和分析系统,可以对全球学者进行文献检索和人才价值评估。用户可以通过关注某些学科领域的顶尖人物而持续追踪该领域的学科进展和研究前沿。经过近期的数据扩容,当前同舟云学术共收录了国内外主流学术期刊6万余种,收集的期刊论文及会议论文总量共计约1.5亿篇,并以每天添加12000余篇中外论文的速度递增。我们也可以为用户提供个性化、定制化的学者数据。欢迎来电咨询!咨询电话:010-8811{复制后删除}0370

www.globalauthorid.com

TOP

Copyright © 2019-2024 北京同舟云网络信息技术有限公司
京公网安备11010802033243号  京ICP备18003416号-3