AbstractHighly crystalline Bi2Te3 based compounds with small grain size were successfully synthesized by flash sintering (FS) method in 10 s at room temperature under suitable current density using Bi, Te and Se powders. The instantaneously generated local Joule heat at grain boundary is regarded as the main reason for the rapid completion of chemical reaction and crystallization. By combining FS synthesis method with spark plasma sintering (SPS), Bi2Te3 based bulk materials with high relative density were fabricated in 10 min. Suitably prolonging sintering temperature and holding time in SPS process can decrease carrier concentration and phonon thermal conductivity, while increasing carrier mobility. Hence, the sample prepared at 753 K for 3 min shows 20% higher ZT value than that of the sample prepared at 723 K for 3 min. Compared with common zone melting or powder metallurgy methods taking several hours by complex operation, this method is time-saving and low cost.
Funder
Research Fund Program of Beijing Information Science & Technology University
National Natural Science Foundation of China
Qin Xin Talents Cultivation Program of Beijing Information Science & Technology University
Publisher
Springer Science and Business Media LLC
Cited by
15 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献