Abstract
Eu3+ doped CaGd4O7 phosphors have been newly synthesized using a solvothermal reaction method and sintered at 1400 °C. The phase, composition, morphologies, and photoluminescent properties of the phosphors have been well characterized by means of
the X-ray diffraction (XRD) patterns, energy dispersive X-ray spectroscopy (EDX), field emission scanning electron microscopy (FE-SEM), photoluminescence (PL) spectroscopy, and decay curves, respectively. The XRD patterns of the as-prepared phosphors confirm their monoclinic structure and
the FE-SEM images reveal flower-like morphology, formed through agglomeration. The calculated size of the crystallites was approximately 83 nm. The photoluminescence excitation (PLE) spectra of CaGd4O7: Eu3+ phosphors consist of a broad band due to the charge
transfer (CT) electronic transition, and several sharp peaks that can be attributed to the f–f transitions of Eu3+ and Gd3+. The PL spectra exhibited a stronger red emission corresponding to the 5D0→7F2 transition.
The CIE chromaticity coordinates of the phosphors were calculated and all the chromaticity coordinates have been placed in the red spectral region. These luminescent powders are expected to have potential applications for white light-emitting diodes (WLEDs) and optical display systems.
Publisher
American Scientific Publishers
Subject
Condensed Matter Physics,General Materials Science,Biomedical Engineering,General Chemistry,Bioengineering
Cited by
10 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献