Feldspathic and Lithium Disilicate Onlays with a 2-Year Follow-Up: Split-Mouth Randomized Clinical Trial

Author:

Saavedra Guilherme de Siqueira Ferreira Anzaloni1ORCID,Tribst João Paulo Mendes1ORCID,Ramos Nathália de Carvalho1ORCID,Melo Renata Marques de1ORCID,Rodrigues Vinícius Anéas2ORCID,Ramos Gabriela Freitas1ORCID,Bottino Marco Antonio1ORCID

Affiliation:

1. UNESP, Brazil

2. FUNVIC, Brazil

Abstract

Abstract The present study was a prospective, controlled, randomized, clinical short-term trial aiming to evaluate the clinical performance of adhesively luted, lithium disilicate and feldspathic glass-ceramics onlays over a period up to 2 years. A total of 11 patients (7 female, 4 male; age range: 18-60 years, mean age: 39 years) were selected for this study. Each patient received a maximum of two restorations per group in a split-mouth-design. LD: Eleven onlays, performed with lithium disilicate-based ceramic (IPS e.max CAD, Ivoclar Vivadent, Schaan, Liechtenstein), and FP: Eleven onlays, performed with feldspathic ceramic (Vita Mark II, Vita Zanhfabrik, Bad Säckingen). Recalls were performed at 2 weeks (baseline = R1), 1 year (R2) and 2 years (R3) after the cementation by three calibrated blinded independent investigators using mirrors, magnifying eyeglasses, probes and bitewing radiographs. The postoperative sensitivity, secondary caries, marginal integrity, marginal discoloration, color match, surface roughness, tooth integrity, and restoration integrity were evaluated. The Friedman test was used to determine if there was a statistically significant difference in time-to-time comparison of the parameters in the ceramics restorations. A total of 95.4% of the restorations were clinically acceptable at the 2-year recall, without a difference for any evaluation parameter for both ceramic materials. Based on the 2-year data, the CAD-CAM onlays manufactured with feldspathic and lithium-disilicate based ceramics showed similar clinical performance.

Publisher

FapUNIFESP (SciELO)

Subject

General Dentistry

Reference22 articles.

1. Self-etching Primers vs Acid Conditioning: Impact on Bond Strength Between Ceramics and Resin Cement;Tribst J;Oper Dent,2018

2. Biaxial flexural strength and Weilbull characteristics of adhesively luted hybrid and reinforced CAD/CAM materials to dentin: effect of self-etching ceramic primer versus hydrofluoric acid etching.;Tribst JPM;J Adhes Sci Technol,2020

3. Lithium Disilicate Crown, Zirconia Hybrid Abutment and Platform Switching to Improve the Esthetics in Anterior Region: A Case Report;Adolfi D;Clin Cosmet Investig Dent,2020

4. Wear of enamel opposing zirconia and lithium disilicate after adjustment, polishing and glazing;Lawson NC;J Dent,2014

5. Fatigue survival and damage modes of lithium disilicate and resin nanoceramic crowns;Ferruzzi F;J Appl Oral Sci,2019

同舟云学术

1.学者识别学者识别

2.学术分析学术分析

3.人才评估人才评估

"同舟云学术"是以全球学者为主线,采集、加工和组织学术论文而形成的新型学术文献查询和分析系统,可以对全球学者进行文献检索和人才价值评估。用户可以通过关注某些学科领域的顶尖人物而持续追踪该领域的学科进展和研究前沿。经过近期的数据扩容,当前同舟云学术共收录了国内外主流学术期刊6万余种,收集的期刊论文及会议论文总量共计约1.5亿篇,并以每天添加12000余篇中外论文的速度递增。我们也可以为用户提供个性化、定制化的学者数据。欢迎来电咨询!咨询电话:010-8811{复制后删除}0370

www.globalauthorid.com

TOP

Copyright © 2019-2024 北京同舟云网络信息技术有限公司
京公网安备11010802033243号  京ICP备18003416号-3