Author:
Butler Elizabeth P.,Fuller Edwin R.,Chan Helen M.
Abstract
AbstractAn experimental approach has been developed using a single-fiber pullout test to measure intrinsic interface properties for ceramic composites. The properties are determined from a pull-out, force-displacement curve, which is directly related to reinforcement toughening via fiber/matrix debonding and frictional pull-out. They were evaluated for a model composite system of continuous SiC fibers with various surface treatments in a borosilicate glass matrix. For the processing conditions used, the interface fracture toughness and the interface frictional shear resistance were found to be 1.0 ± 0.5 J/m2 and 3.3 ± 0.6 MPa, respectively, for as-received fibers. Experiments conducted with long embedded fiber lengths allowed the shear resistance to be deconvolved into an interface friction coefficient of 0.05 ± 0.01 and an initial fiber-clamping pressure of 65 ± 6 MPa. Nitric acidwashed fibers gave an increased interface toughness of 3.6 ± 0.1 J/m2 and friction coefficient of 0.08 ± 0.02, but nearly the same initial clamping pressure, 72 ± 12 MPa. Calculations of the clamping pressure from the fiber/matrix thermal expansion mismatch and from stress birefringence measurements in the glass were in general agreement with this value.
Publisher
Springer Science and Business Media LLC
Cited by
19 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献