AbstractThe tensile properties of SiC fiber, Ti Al+Nb and SiC/Ti3Al+Nb composite have been determined from 300 to 1365K. The Composite results compared favorably to rule-of-mixtures (ROM) predictions in the intermediate temperature regime of 475 to 700K. Deviations from ROM are discussed. Composite tensile results were compared on a strength/density basis to wrought superalloys and found to be superior. Fiber-matrix compatibility was characterized for the composite at 1250 and 1365K for 1 to 100 hours.