Abstract
Ni/8 mol% Y2O3-stabilized zirconia cermets are used in thin-film electrolyte solid-oxide fuel cells as support substrates. Rapid oxidation of the metallic Ni can cause failure of the substrate and of the whole system. The rate of Ni oxidation in air and in an inert atmosphere containing water vapor was determined as a function of temperature between 500 and 950 °C. A logarithmic rate law describes the oxidation kinetics in air, whereas a linear rate law fits the first branch of the curve of the experimental data in a humidified inert atmosphere. The substrate exhibits no significant mechanical degradation after uniform oxidation under moderate conditions. However, the observed bending of the samples after oxidation in humidified argon, due to the nonuniform oxidation, can cause damage to fuel cell
Publisher
Springer Science and Business Media LLC
Subject
Mechanical Engineering,Mechanics of Materials,Condensed Matter Physics,General Materials Science
Cited by
67 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献