Chiang C. K.,Wong-Ng W.,Cook L. P.,Schenck P. K.,Lee H. M.,Brody P. S.,Bennett K. W.,Rod B. J.
Abstract
AbstractPZT thin films were prepared by pulsed laser deposition on unheated Ptcoated Si substrates. As deposited, the films were amorphous. Films crystallized at 550 - 600 °C to produce predominantly crystalline ferroelectric PZT. Crystallization of the amorphous material was accompanied by a linear shrinkage of ∼2 %, as manifested in development of cracks in the film. Spacing, width and morphology of larger cracks followed a regular progression with decreasing film thickness. For film thicknesses less than 500 runm, much of the shrinkage was taken up by small, closely-spaced cracks of local extent. Implications for measurement of PZT thin film ferroelectric properties and processing are discussed.
Publisher
Springer Science and Business Media LLC
Reference5 articles.
1. Lead Zirconate-Titanate Thin Films Prepared by the Laser Ablation Technique
2. Microstructural Changes During Processing of Laser-Deposited BaTiO3 and Pzt Thin Films
3. 2. Brody P.S. , Rod B.S. , Benedetto J.M. , Bennett K.W. , Cook L.P. , Schenck P.K. , Chiang C.K. and Wong-Ng W. , Proc. Seventh Intl Symp. on Applic. of Ferroelectrics, Univ. III, Urbana-Champaign, IL., (1990).
4. Proc. Symposium on Beam Solid Interaction: Physical Phenomena;Schenck;Mat. Res. Soc.,1990