Author:
Inagaki Y.,Sakata H.,Furuya H.,Idemitsu K.,Arima T.,Banba T.,Maeda T.,Matsumoto S.,Tamura Y.,Kikkawa S.
Abstract
ABSTRACTThe objective of this study is to evaluate the effects of water redox conditions and of the presence of iron corrosion products (magnetite) on the release of actinides from HLW glasses. Static corrosion tests were performed on a simulated HLW glass doped with Pu and Np in deionized water in the presence of magnetite under oxidizing and reducing conditions. The tests under oxidizing conditions were performed in air, while the tests under reducing conditions were performed in mixed gas (Ar+5%H2) atmosphere.The following results were obtained: (1) The presence of magnetite enhances formation of colloids containing Pu and Np in the leachates under both redox conditions. (2) Redox conditions have no remarkable influence on the release of Pu. (3) The reducing conditions combined with the presence of magnetite cause a decrease in the concentrations of Np dissolved species, which is probably the result of the reduction of Np(V) to Np(IV) at the magnetite surface.
Publisher
Springer Science and Business Media LLC
Cited by
19 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献