Author:
Spencer Nicholas D.,Peders Thorvald S.,Baer Matthew B.
Abstract
The effect of different drying and calcination methods on the ultimate particle size of YBa2Cu3O7 (Y-123) has been investigated. The starting material was a tetramethylammonium (TMA) carbonate-precipitated slurry. Spray-drying the slurry after filtering and reslurrying (to remove residual TMA) was most effective in the ultimate formation of finely divided Y-123. The morphology of the spray-dried powder could be preserved by calcining in very low total pressures of flowing oxygen. When a slurry with 0.16% solids content was spray dried, and this powder calcined at 750 °C in 2 Torr of flowing oxygen, a Y-123 powder of mean particle size 0.74 μm (66% submicron) was obtained.
Publisher
Springer Science and Business Media LLC
Subject
Mechanical Engineering,Mechanics of Materials,Condensed Matter Physics,General Materials Science
Reference8 articles.
1. Freestanding thick films of YBa2Cu3O6.9 by screenprinting techniques
2. 3 Spencer N. D. , Pan W. H. , and Rudesill J. A. , Eur. Patent Applic. 0306973, 1988.
3. 6 Spencer N. D. , Chemistry of Materials (in press).
4. Synthesis of phase-pure orthorhombic YB2Cu3Ox under low oxygen pressure
5. 4 Bunker B. C. , Lamppa D. L. , and Voigt J. A. , Patent U. S. 4 839 339, 1989.
Cited by
5 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献