Affiliation:
1. Forschungszentrum Jülich, Institut für Energie- und Klimaforschung, 52425 Jülich, Germany
Abstract
Plasma-facing materials (PFMs) in the ITER divertor will be exposed to severe conditions, including exposure to transient heat loads from edge-localized modes (ELMs) and to plasma particles and neutrons. Tungsten is the material chosen as PFM for the ITER divertor. In previous tests, bubble formation in ITER-grade tungsten was detected when exposed to fusion relevant conditions. For this study, ITER-grade tungsten was exposed to simultaneous ELM-like transient heat loads and D/He (6%) plasma in the linear plasma device PSI-2. Bubble formation was then investigated via SEM micrographs and FIB cuts. It was found that for exposure to 100.000 laser pulses of 0.6 GWm−2 absorbed power density (Pabs), only small bubbles in the nanometer range were formed close to the surface. After increasing Pabs to 0.8 and 1.0 GWm−2, the size of the bubbles went up to about 1 µm in size and were deeper below the surface. Increasing the plasma fluence had an even larger effect, more than doubling bubble density and increasing bubble size to up to 2 µm in diameter. When using deuterium-only plasma, the samples showed no bubble formation and reduced cracking, showing such bubble formation is caused by exposure to helium plasma.
Funder
European Union via the Euratom Research and Training Programme
Cited by
1 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献