Abstract
This research investigates the performance of medium density fiberboard (MDF) with respect to hot press parameters. The performance of the board, type of glue, and production efficiency determine the optimum temperature and pressure for hot pressing. The actual temperature of the hot press inside the MDF board determines the properties of the final product. Hence, the optimal hot press parameters for the desired product are experimentally obtained. Moreover, MDF is experimentally investigated in terms of its vertical density profile, bending, and internal bonding under the various input parameters of temperature, pressure, cycle time, and moisture content during the manufacturing process. The experimental study is carried out by varying the temperature, pressure, cycle time, and moisture content in the ranges of 200–220 °C, 145–155 bar, 260–275 s, and 8–10%, respectively. Consequently, the optimum input parameters of a hot-pressing temperature of 220 °C, pressure of 155 bar, cycle time of 256 s, and moisture content of 8% are identified for the required internal bonding (0.64 N/mm2), bending (32 N/mm2), and increase in both the core and peak density of the vertical density profile as per the ASTM standard.
Subject
Fluid Flow and Transfer Processes,Computer Science Applications,Process Chemistry and Technology,General Engineering,Instrumentation,General Materials Science
Reference27 articles.
1. Properties of Medium Density Fiberboard Based on Bagasse Fibers
2. Effects of thermal treatment of rubber wood fiber on physical and mechanical properties of MDF;Ayrilmis;J. Trop. For. Sci.,2011
3. Wheat straw as raw material for manufacture of straw MDF;Halvarson;BioResources,2010
4. MPOB TT No. 493.Optimum parameters for the production of MDF using 100% oil palm trunks;Ibrahim;MPOB Inf. Ser.,2006
5. Mechanical and physical properties of medium density fiberboard panels laminated with thermally compressed veneer
Cited by
2 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献