Abstract

The accelerated weathering of flax and miscanthus fibers possessing distinct chemical compositions was investigated. The chosen fibers included raw, extractive-free (EF) and delignified samples (x3), alone and used as fillers in a stabilized polypropylene blue matrix (PP). Modifications in both color and the chemical composition of the fibers throughout the weathering process under ultraviolet (UV) light were meticulously tracked and analyzed by spectrophotometry and attenuated total reflectance with Fourier-transform infrared spectroscopy (ATR-FTIR). The inherent nature and composition of the selected fibers led to varied color-change tendencies. Raw and EF flax fibers exhibited lightening effects, while raw and EF miscanthus fibers demonstrated darkening effects. Extractives exhibited negligible influence on the color alteration of both flax and miscanthus fibers. This disparity between the fibers correlates with their respective lignin content and type, and the significant formation of carbonyl (C=O) groups in miscanthus. Better stability was noted for delignified flax fibers. A comparative study was achieved by weathering the PP matrix containing these various fibers. Contrary to the weathering observations on individual fibers, it was noted that composites containing raw and EF flax fibers exhibited significant color degradation. The other fiber-containing formulations showed enhanced color stability when compared to the pure PP matrix. The study highlights that the UV stability of composites depends on their thermal history. As confirmed by thermogravimetric analysis (TGA), fiber degradation during extrusion may affect UV stability, a factor that is not apparent when fibers alone are subjected to UV aging.

Funder

BPI France

Publisher

MDPI AG

同舟云学术

1.学者识别学者识别

2.学术分析学术分析

3.人才评估人才评估

"同舟云学术"是以全球学者为主线,采集、加工和组织学术论文而形成的新型学术文献查询和分析系统,可以对全球学者进行文献检索和人才价值评估。用户可以通过关注某些学科领域的顶尖人物而持续追踪该领域的学科进展和研究前沿。经过近期的数据扩容,当前同舟云学术共收录了国内外主流学术期刊6万余种,收集的期刊论文及会议论文总量共计约1.5亿篇,并以每天添加12000余篇中外论文的速度递增。我们也可以为用户提供个性化、定制化的学者数据。欢迎来电咨询!咨询电话:010-8811{复制后删除}0370

www.globalauthorid.com

TOP

Copyright © 2019-2024 北京同舟云网络信息技术有限公司
京公网安备11010802033243号  京ICP备18003416号-3